Flow Pattern And Temperature Distribution Of Molten Glass In A Forhearth

The temperature distribution of glass in a forehearth was calculated using a mathematical model and results were compared using a mathematical model and results were compared with experimental data. A physical model experiment was also carried out. It was found that the glass flowed forward with a rotating motion and the shape of the velocity distribution was equally parabolic.

Author
T. Mishioka Et Al
Origin
Unknown
Journal Title
Reports Of The Research Laboratory Ashai Glass Co Ltd 1971 21 (1) 1-17
Sector
Primary Papers
Class
PP 563

Request article (free for British Glass members)

Flow Pattern And Temperature Distribution Of Molten Glass In A Forhearth
Reports Of The Research Laboratory Ashai Glass Co Ltd 1971 21 (1) 1-17
PP 563
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.