Flow Microcalorimetric Estimation Of Energy Changes During Surface Reactions Of Glass Powders With Aqueous Media

Flow microcalorimetry has been used for an investigation of the nature of glass surfaces, i.e. fused silica and a fluorozirconate glass.

Author
J P Fletcher Et Al
Origin
University Of Arizona
Journal Title
J Am Ceram Soc 1989 72 9 1744-1746