Float Furnace Repair Projects: Plan Big, Rebuild More

In this article the author describes how the planning of a float glass furnace cold repair project is imperative, in terms of prioritising staff safety, minimising the risk of problems during start up and optimising the downtime by carrying out as much maintenance and repair work as possible on the rest of the plant's operations.