Float Chamber Effects On Redox Conditions

In this article the authors describe investigations into the influence of float chamber conditions on the redox condition of glass and its optical characteristics.

Author
H Hessenkemper & K Al Hamdan
Origin
Tu Bergakademie Freiberg
Journal Title
Glass Worldwide 30 July-Aug 2010 20, 22
Sector
General
Class
G 3753