Flexural Creep Behaviour Of Al203 Doped Sic At Elevated Temperatures In Air (Tables In English/Text In Japanese)

Creep tests in four point flexural loading configuration in air employing applied stresses of 100-350 MPa at temperatures of 1400, 1500 and 1600 deg C were performed on Al203 doped SiC.