Flexible Thin Glass Substrates For Durble And Cost Effective Thin Film Solar Cells

The recent 2007 "Strength in Glass" contest sponsored by GMIC saw as its winner among 47 entries from 28 universities in five countries. The article describes the most credible, practical and potentially realisable application for a theoretical strong glass material.

Author
A Dellert
Origin
Fredrich Alexander University, Germany
Journal Title
Glass-Tech Int 1/2008 97-100
Sector
Flat glass
Class
F 2499