Flexible Glass To Challenge Lcds In Electronic Devices

Corning Inc recently announced it has developed a flexible glass substrate that can be used for printed electronics applications. The glass manufacturer says the product performs like glass and is as flexible as plastic. The display is 75 micrometers thick and wholly protected by plastic. According to Technology Review, Corning currently su