Flaw Generation During Constrained Sintering Of Metal-Ceramic And Metal-Glass Multilayer Films

Sintering of symmetrical multilayer films has been studied theoretically and experimentally. There is evidence that the metal layer deforms plastically when placed in tension by differential sintering.