Flat Jet Oxy-Fuel Burner For Uniform Heat Transfer

This paper outlines the background, features and performance of a novel oxy-fuel burner for glass melting applications. Flame characteristics such as controllable heat transfer rates and NOx formation rates have been optimised using Computational Fluid Dynamic (CFD) techniques and contrary to traditional axisymmetric oxy-fuel systems, "flat" flames have been established using proprietary burner technology to give uniform heat transfer rates. Some results from a research furnace installation are also presented here.

Author
Dr L T Yap
Origin
Boc Group Tech Centre, Usa
Journal Title
Glass 71 6 1994 199, 201-202
Sector
General
Class
G 1139

Request article (free for British Glass members)

Flat Jet Oxy-Fuel Burner For Uniform Heat Transfer
Glass 71 6 1994 199, 201-202
G 1139
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
10 + 8 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.