The Flat Glass Industry In China

Sustainable and rapid development of the Chinese economy has propelled the fast development of China's glass industry. In 2006, overall output of flat glass in China reached 23.3M/tons, accounting for around 42% of the world's total. China requires advanced technologies and equipment, and its glass production techniques and processing machinery have reached a fairly high level. This article describes the current situation within the Chinese flat glass sector.