Flame Spectrophotometric Analysis Of Glasses And Ores: I Lithium, Sodium, Potassium, Rubidium And Cesium.

The alkali elements in a wide range of glass and feldspar ore compositions can be rapidly determined with the flame spectrophotometer without making chemical separations. Flame photometer response to lithium, sodium, and potassium seems little affected by the presence of many of the glass constituents in concentration ranges found in commercial glasses.

Author
Jp Williams And Pb Adams
Origin
Unknown
Journal Title
Jacs 37 7 1954 306-311
Sector
Primary Papers
Class
PP 1375

Request article (free for British Glass members)

Flame Spectrophotometric Analysis Of Glasses And Ores: I Lithium, Sodium, Potassium, Rubidium And Cesium.
Jacs 37 7 1954 306-311
PP 1375
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
9 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.