Flame Particle Seeding With Oxygen Enrichment For Nox Reduction And Increased Efficiency

An improved method of gas firing, involving flame particle seeding for reducing NOx emissions, is outlined.

Author
M L Joshi Et Al
Origin
Combustion Tec Inc, Southern California Gas Co
Journal Title
Glass June 1991 212-213
Sector
General
Class
G 626