Flaking Of Commercial Glass Containers

The formation of bloom and flaking during the corrosion of the inside surface of a glass container are discussed to understand how to produce containers of acceptable chemical durability. Glass composition, manufacturing conditions, storage conditions, and bottle washing and filling conditions all influence the problem of weathering and the tendency of containers to bloom or flake before use by the consumer. Means of preventing weathering, such as hot end surface treatments, are outlined, as are methods for cleansing containers already weathered.

Author
M Brungs & A Grigg
Origin
Australian Consolidated Industries, Sydney
Journal Title
Glass Technology 16 6 December 1975 135-138
Sector
Primary Papers
Class
PP 99

Request article (free for British Glass members)

Flaking Of Commercial Glass Containers
Glass Technology 16 6 December 1975 135-138
PP 99
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 9 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.