First Class Safety In Is Machine Operation

According to the authors of this article, high productivity in glass container production requires maximum safety. Based on a presentation delivered at the 12th ESG Conference in Parma, this article discusses a series of equipment innovations to protect employees and equipment.

Author
M Zeigler & W Seidensticker
Origin
Heye International
Journal Title
Glass Worldwide Nov-Dec 2014 52, 54
Sector
Container glass
Class
C 5234