Finiate Element Calculation Of Refractive Index In Optical Glass Undergoing Viscous Relaxation And Analysis Of The Efefcts Of Cooling Rate And Material Properties

In this research, a methodology based on a numerical simulation model is presented to predict refractive index change introduced to two low Tg optical glasses, namely, P-SK57 and P-LASF47, by cooling. To model the structural relaxation behaviour of the glass around glass transition temperature, the Tool-Narayanaswamy-Moynihan (TNM) model is used. In addition, the fictive temperature of the glass samples during cooling is discussed. The effect of cooling rate on the fictive temperature of the glass samples is also presented. The study demonstrated that finite element method is capable of predicting refractive index of optical glass undergoing viscous relaxation.

Author
L Su & A Y Yi
Origin
Ohio State University, Usa
Journal Title
Int J Appl Glass Sci 3 3 2012 263-274
Sector
Special Glass
Class
S 3936

Request article (free for British Glass members)

Finiate Element Calculation Of Refractive Index In Optical Glass Undergoing Viscous Relaxation And Analysis Of The Efefcts Of Cooling Rate And Material Properties
Int J Appl Glass Sci 3 3 2012 263-274
S 3936
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.