Finely Disperse Heat-Resistant Refractories Based On Technogenic Materials

Investigation results of application of carborundum plate scrap in the production of finely disperse heat-resistant saggers by the slip casting method are presented. The main physicochemical properties of the considered mixtures based on plate scrap are not inferior to those of mixtures based on silicon carbide. Experimental lots of saggers of different shapes exhibited good service properties. At the same time, the production cost of saggers is reduced to approximately one-third.

Author
V P Sivov & P V Sivov
Origin
Unknown
Journal Title
Glass & Ceramics 56 9-10 1999 308-311
Sector
Refractories
Class
R 395

Request article (free for British Glass members)

Finely Disperse Heat-Resistant Refractories Based On Technogenic Materials
Glass & Ceramics 56 9-10 1999 308-311
R 395
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
10 + 9 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.