Fine-Grained Silicon Carbide Ceramics With Oxynitride Glass

By using an oxynitride glass composition from the Y-Mg-Si-Al-0-N system as a sintering additive, the effect of atmosphere on densification was investigated during the liquid-phase sintering of SiC, and the resulting microstructure and mechanical properties of the sintered and subsequently annealed materials were investigated.

Author
Y Kim & M Mitomo
Origin
Univ Seoul, Korea & Inst Res Inorg Mat, Japan
Journal Title
J Am Ceram Soc 82 10 1999 2731-2736
Sector
Special Glass
Class
S 1788

Request article (free for British Glass members)

Fine-Grained Silicon Carbide Ceramics With Oxynitride Glass
J Am Ceram Soc 82 10 1999 2731-2736
S 1788