Finding The Formula For The Tin Bath

The development of appropriate formulations for tin bath blocks has been a story of trial and error: as problems were found, forumlations changed only to create other problems.

Author
Un-named
Origin
Dsf Refractories, Derbyshire, Uk
Journal Title
Glass Industry 80 11 1999 28