Fibre-Matrix Interface Properties Of Single-Fibre Microcomposites As Measured By Fibre Pushin Tests

Fibre pushin tests have been performed on single-fibre microcomposite specimens embedded in glass. The interface properties determined were in agreement with those previously determined by two methods from tensile tests on microcomposites. The uncertaintaies in the interface properties calculated from the microcomposite pushin tests were not found to benefit from the superior alignement of the microcomposite specimens, as compared to literature results from composites specimens.

Author
R J Kerans Et Al
Origin
Usaf Wright Lab Materials, Ohio, Usa
Journal Title
J Am Ceram Soc 80 2 1997 506-508
Sector
Glass Fibre
Class
GF 169

Request article (free for British Glass members)

Fibre-Matrix Interface Properties Of Single-Fibre Microcomposites As Measured By Fibre Pushin Tests
J Am Ceram Soc 80 2 1997 506-508
GF 169
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.