Fiber, Whisker And Particulate Reinforced New Glass-Ceramic Matrix For Innovative Composites

In this article a new CMAS glass-ceramic matrix, which separates diopside celsian and hexacelsian, is reinforced with Al2O3 chopped fibers, SiC whiskers and particulate, and AIN particulate. The reactivity towards the formation of an interface between the reinforcement and the matrix is analysed by microstructural characterisation: XRD, SEM and Vickers microhardness testing, in order to anticipate the mechanical behaviour.

Author
L Barbieri Et Al
Origin
Unknown
Journal Title
Rivista Della Staz Sper Vetro 23 6 1993 293-295
Sector
Glass Ceramics
Class
GC 159

Request article (free for British Glass members)

Fiber, Whisker And Particulate Reinforced New Glass-Ceramic Matrix For Innovative Composites
Rivista Della Staz Sper Vetro 23 6 1993 293-295
GC 159
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 12 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.