Feldspar & Nepheline Syenite At The Mercy Of Glass Markets

The competition for markets between feldspar and nepheline syenite with each other and with other materials is discussed with particular reference to the United States, where the glass industry uses about 54% of total feldspar, and 70% of total nepheline syenite, production.

Author
J Burger
Origin
Unknown
Journal Title
Industrial Minerals August 1990 21-33
Sector
General
Class
G 458