Feedforward-Feedback Control Of Gas Fired Glass Forehearths

The development of algorithms for control of the surface temperature of the glass in a gas fired forehearth is described.

Author
H Bartlett, A K Kochlaar
Origin
University Of Bradford
Journal Title
Glass Technology 1988 29 1 35-42
Sector
Container glass
Class
C 41