Fea Studies Of Impact Loads On Nnpb Refillable Bottles

In a previous study, the internal pressure and vertical load performance of refillable bottles was evaluated through computer stress analysis. The evaluation compared the same bottle designs made by both the NNPB process and the blow-and-blow process using two different approaches. In this article, the author's discuss impact load considerations when using NNPB forming technology for refillable beer bottles.