Faulty Pet Bottles Leave Bad Taste In Mouth!

Finnish alcoholic beverage manufacturer Altia has found the cause of the fault in flavour in its Sisuviina spirit. Alcohol retailer Alko withdrew thousands of litres of the spirit from the market in the beginning of March 2009 because of a bad taste. According to Altia, the problem was caused by faulty PET bottles. The one-litre bottles had been bought from a European supplier.