Failure Of Glass With Subthreshold Flaws

A fracture mechanics model for failure of glass with subthreshold indentation flaws has been developed. Results of experiments with bare fused silica fibres with indentation subthreshold flaws in inert and fatigue (water) environments were in good agreement with the predictions by the model.