Factors For Calculating The Properties Of Soda-Lime Glasses And Their Use In The Design Of Container Glasses (Portuguese)

Factors are presented, together with assessments of their accuracy, for calculating the effect of various oxides on the viscosity, chemical durability, density and thermal expansion coefficient of container-type compositions.

Author
A Smrcek, J Rysavy
Origin
Sklo-Union - Obas, Vusu
Journal Title
Vidro November/December 1989 15-16
Sector
Container glass
Class
C 269