Fabrication Of Nanoscale Glass Fibers By Electrospinning

We report the experimental realization of glass nanofibers by electrospinning directly from a melt, demonstrating the viability of electrospinning fibers from non-polymer materials with high melting temperatures and higher surface tensions. The nanofiber material (B2O3) is molten on the tip of a gold wire, and voltage applied to the tip causes a jet to form, resulting in solid glass fibers with diameters of 100 nm.

Author
M Praeger Et Al
Origin
University Southampton, Uk
Journal Title
Applied Physics Letters 100, 063114 (2012)
Sector
Glass Fibre
Class
GF 668

Request article (free for British Glass members)

Fabrication Of Nanoscale Glass Fibers By Electrospinning
Applied Physics Letters 100, 063114 (2012)
GF 668