Fabrication Of Intrinsically Low Nonlinearity Glass Optical Fibres

Optical nonlinearities limit attempts to increase power scaling in high-energy laser systems. Oxyfluoride glass optical fibres offer one potential materials solution.

Author
M Cavillon Et Al
Origin
Comset, Usa
Journal Title
Am Ceram Soc Bull 97 4 2018 34-35
Sector
Glass Fibre
Class
GF 754