Fabrication And Ultraviolet Absorption Of Sol-Gel-Derived Germanium Oxide Glass Thin Films

Germanium oxide glass thin films were prepared by the sol-gel method and annealed under reduced atmosphere to create more oxygen-deficient defects. The densification and crystallization were examined depending on sintering and annealing conditions. Thus, homogeneous germanium oxide thin films with a high content of oxygen vacancies were fabricated. Ultraviolet absorption and oxygen vacancies of the films were investigated as a function of annealing temperature and time. Optical absorption in the 5-eV region due to the formation of oxygen vacancies is enhanced with increasing annealing temperature and time. The formation energy of oxygen vacancies is calculated to be about 1.0 eV.

Author
J H Jang Et Al
Origin
Lomc, Korea
Journal Title
J Am Ceram Soc 83 6 2000 1356-1360
Sector
Special Glass
Class
S 1958

Request article (free for British Glass members)

Fabrication And Ultraviolet Absorption Of Sol-Gel-Derived Germanium Oxide Glass Thin Films
J Am Ceram Soc 83 6 2000 1356-1360
S 1958
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.