Fabrication And Mechanical Properties Of Ni-Nb Metallic Glass Particle-Reinforced Al-Based Metal Matrix Composite

Ni70Nb30 metallic glass powders were prepared by mechanical alloying and subsequently combined with A1 in order to form a metallic glass particle-reinforced A1-based metal matrix composite sintered below the melting temperature of Al by using the powder metallurgy method. The Young's modulus, yield strength and ultimate strength are all higher than for single-phase pure A1.

Author
P Yu Et Al
Origin
Technical Unviersity Dargnstadt, Germany
Journal Title
Scripta Materialia 54 2006 1445-1450
Sector
Special Glass
Class
S 3083

Request article (free for British Glass members)

Fabrication And Mechanical Properties Of Ni-Nb Metallic Glass Particle-Reinforced Al-Based Metal Matrix Composite
Scripta Materialia 54 2006 1445-1450
S 3083
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.