Fabrication And Mechanical Properties Of Silicon Carbide-Silicon Nitride Composites With Oxynitride Glass

A microstructure that consisted of uniformly distributed, elongated B-Si3N4 grains, equiaxed B-SiC grains, and an amorphous grain-boundary phase was developed by using B-SiC and a-Si3N4 powders.