Fabrication And Efficient Infrared-To-Visible Upconversion In Transparent Glass Ceramics Of Er-Yb Co-Doped Caf2 Nano-Crystals

Transparent glass ceramics containing CaF2 nano-crystals co-doped with Er-Yb were developed by heat treatment of glasses in the system SiO2-Al2O3-Caf2-LnF3 (Ln=Er, Yb). The crystal size of CaF2 increased with increasing heat-treatment temperature. Up conversion emission intensities at 660 and 540 nm increased dramatically with increasing heat-treatment temperature. The cathode luminescence mapping indicates that the visible Er-luminescence arises mainly from the precipitated CaF2 nano-crystals with a phonon energy lower than that of a silicate matrix. It is concluded that both Er and Yb were concentrated in the CaF2 nano-crystals, and the quantum efficiency of Er3+ luminescence and the energy transfer efficiency from Yb3+ were considerably improved after ceramization.

Author
Y Kishi Et Al
Origin
Kyoto University, Japan
Journal Title
J Am Ceram Soc 88 12 2005 3423-3426
Sector
Glass Ceramics
Class
GC 649

Request article (free for British Glass members)

Fabrication And Efficient Infrared-To-Visible Upconversion In Transparent Glass Ceramics Of Er-Yb Co-Doped Caf2 Nano-Crystals
J Am Ceram Soc 88 12 2005 3423-3426
GC 649
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.