Extrapolation Of Experimental Results For The Determination Of Light Transmittance Of Diffusing Glazing

Many diffusing transparent materials require the use of large integrating spheres for accurate transmittance measurements. Nevertheless, measurements on materials with high diffusing behaviour and remarkable thickness require sample ports (and consequently integrating sphere diameters) large enough to collect the whole transmitted radiation through the sample. This solution cannot always be achieved for economical and technical reasons. In this paper a solution to this problem is offered.

Author
A Maccari Et Al
Origin
Unknown
Journal Title
Riv Staz Sper Vetro 28 6 1998 265-270
Sector
Special Glass
Class
S 1649

Request article (free for British Glass members)

Extrapolation Of Experimental Results For The Determination Of Light Transmittance Of Diffusing Glazing
Riv Staz Sper Vetro 28 6 1998 265-270
S 1649
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.