Extraction Of Silicon Dioxide From Waste Coloured Glasses By Alkali Fusion Using Sodium Hydroxide

A process for extraction of Si02 from waste coloured glasses by alkali fusion using NaOH was investigated. In this study, glass waste coloured bottles of green, blue, brown or black were selected as samples of waste glasses. These coloured bottles were qualitatively confirmed to contained elements of Na, Mg, Al, Si, K, Ca, Ti, Mn, Fe and Cu from energy dispersive x-ray spectroscopic analysis. The condition for alkali fusion of NaOH and the waste glasses was optimised, i.e. for each bottle, the composition was NaOH: crushed glass bottle=90:10 mass%, melting temperature was 500 deg C and melting time was 2 hours. For each waste coloured bottle, the sodium silicate solution was prepared by using the sodium silicate obtained by alkali fusion. After mixing HCl with the solution, Si(OH)4 was then precipitated by boiling the solution which became a very strong acid.

Author
H Mori
Origin
Unknown
Journal Title
J Ceram Soc Japan 111 6 2003 376-381
Sector
Container glass
Class
C 2199

Request article (free for British Glass members)

Extraction Of Silicon Dioxide From Waste Coloured Glasses By Alkali Fusion Using Sodium Hydroxide
J Ceram Soc Japan 111 6 2003 376-381
C 2199
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.