External Over-Coating Of The Glass Bath

During the campaign life of a furnace, either designed or extended, it is inevitable that external over-coating of the melting end glass bath will be required at some stage. In this article, Michael Horsfield considers the application of external over-coating to the furnace glass bath and the need for continuous monitoring. He concludes that over-coating of the glass bath primary refractory can retain a particular encountered problem and extend furnace campaign life, However, it can also introduce added complications if the over-coated positions are not monitored on a scheduled basis.

Author
M Horsfield
Origin
Dismatec, Uk
Journal Title
Glass Worldwide 30 2010 34, 36-37
Sector
General
Class
G 3757

Request article (free for British Glass members)

External Over-Coating Of The Glass Bath
Glass Worldwide 30 2010 34, 36-37
G 3757
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.