Extending The Life Of Fused Cast Ceramics

Since the 1990s, development of a precious metal coating technology has been ongoing. In recent years, the research focus has shifted from the consumable refractories (o-rings, tube stirrers etc) to fused cast AZS furnace blocks. This has been driven by glass manufacturers looking for a solution to excessive refractory wear. This wear impacts both furnace life and glass quality. Until recently, the coating could only be applied to machined fused cast AZS surfaces. This paper details the latest innovation of applying the coating to the "as-cast" surface of fused cast AZS blocks and includes micro-graphical analysis and comparison of "as-cast" and "machined" AZS surfaces, details of the latest innovations in the laser pre-treatment process, and results of a three-year plant trial.

Author
R Mcgrath & J Crowe
Origin
Johnson Matthey Plc, Uk
Journal Title
77 Conf On Glass Problems 2017 171-177
Sector
Refractories
Class
R 882

Request article (free for British Glass members)

Extending The Life Of Fused Cast Ceramics
77 Conf On Glass Problems 2017 171-177
R 882
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.