Extending The Life Of Fused Cast Ceramics

Since the 1990's, development of precious metal coating technology (ACT coatings) has been on-going. In recent years the research focus has shifted from consumable refractories to fuse cast AZS furnace blocks. This has been driven by glass manufacturers looking for a solution to excessive refractory wear. This wear impacts both furnace life and glass quality. This paper details the latest innovation of applying the coating to the "as-cast" surface of fused cast AZS blocks and includes micro-graphical analysis and comparison of "as-cast" and "machine" AZS surfaces, details of the latest innovations in the laser pre-treatment process, and results of a three year plant trial.

Author
R Mcgrath, J Crowe
Origin
Johnson Matthey, Uk
Journal Title
77 Conf On Glass Problems 38 1 2017 171-177
Sector
Refractories
Class
R 905

Request article (free for British Glass members)

Extending The Life Of Fused Cast Ceramics
77 Conf On Glass Problems 38 1 2017 171-177
R 905
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
9 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.