Experimental Methodology For The Determination Of The Heat Transfer Coefficient At The Glass/Mould Interface (In French)

A new laboratory testing for the analysis of glass/mould contact is proposed. The various components of the new installation and their kinematics, the choice of the measuring instruments and their accurate location are described. From the temperature evolution in the contact area, coupling inverse method and thermal computations by finite difference method leads to the transient estimation of the heat exchange coefficient at the glass/mould interface.

Author
P Moreau Et Al
Origin
University Of Valenciennes
Journal Title
Verre 9 2 April 2003 24-27
Sector
Container glass
Class
C 2070

Request article (free for British Glass members)

Experimental Methodology For The Determination Of The Heat Transfer Coefficient At The Glass/Mould Interface (In French)
Verre 9 2 April 2003 24-27
C 2070
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.