Experimental And Numerical Study Of Optimum Thickness Of Porous Silica Transition Layer In Aeronautic Laminated Glass

The application of a porous silica (PS) transition layer in an inorganic-organic aeronautic laminated glass can effectively solve the material failure caused by the performance difference of the inorganic-organic materials. The effect of porous silica transition layer thickness on the mechanical and optical properties of laminated glass was investigated. The microstructure of the porous silica transition layer was analyzed by scanning electron microscopy. The film thickness was verified using a step profiler. The failure strength of laminated glass with the porous silica transition layer was tested by a universal testing machine. Finite element modeling of laminated glass with the porous silica transition layer was performed by ANSYS software. Tensile stress between the porous silica and the polyurethane was simulated for different porous silica film thicknesses. Experimental and theoretical results indicated that with the increasing the thickness of the transition film, the failure stress of the laminated glass increased. Improvements in the mechanical properties of the laminated glass are saturation at a PS thickness of approximately 3.8 μm.

Author
Z Feng Et Al
Origin
Nanchang Hangkong University
Journal Title
Materials Design 121 May 2017 367–372
Sector
Flat glass
Class
F 3972

Request article (free for British Glass members)

Experimental And Numerical Study Of Optimum Thickness Of Porous Silica Transition Layer In Aeronautic Laminated Glass
Materials Design 121 May 2017 367–372
F 3972
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.