Experiences With An Oxygen-Fired Container Glass Furnace With Silica Crown - 14 Years - A World Record?

Fourteen years ago the introduction of oxy-fuel combustion in glass melting technology in the Dutch glass industry began. This paper refers to the first oxy-fuel furnace in The Netherlands, and the experiences with a silica crown. First, an explanation about the environmental legislation in The Netherlands is given, which lead to the installation of this first oxy-fuel furnace. This is followed by a description of this first full scale oxy-fuel implementation and the experiences with emission reduction, energy consumption, refractory wear and glass composition in this furnace.

Author
J J Schep
Origin
O-I, The Netherlands
Journal Title
69Th Conf On Glass Problems (Cesp 30 1 2009) 3-11
Sector
General
Class
G 3855

Request article (free for British Glass members)

Experiences With An Oxygen-Fired Container Glass Furnace With Silica Crown - 14 Years - A World Record?
69Th Conf On Glass Problems (Cesp 30 1 2009) 3-11
G 3855
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.