Excimer Laser Processing Of Bk7 And Bgg31 Glasses

This paper examines large-area excimer laser processing of BK7 and BGG31 glasses for laser etching and laser-assisted metallization. A qualitative thermal model describing laser etching of glass in the ablation retion is discussed.