Examination Of Industrial Practice Of Ceramic Glaze Making With Emphasis On Particle Size Distribution

This article examines the existing industrial practice of glaze making with emphasis on particle size and particle size distribution of glazes. The importance of fine grinding affecting reduction in particle size on lowering the maturing temperature has been clearly established taking sanitaryware glaze as an example. Studies on gloss and thermal expansion of glazes having varied particle size distribution have also been carried out. An attempt has also been made to redefine the particle size distribution, which could produce better results. It has been found that the ceramic glazes can safely be ground to d100 of 20 um from the existing industrial practice of maintaining d100 in the range of 45 to 32 um. It has also been established that, along with the increase in particle fineness, not only the maturing temperature of glaze reduced by ~80 degrees C but also the maturing range of sanitaryware glaze significantly increases from 1150 degrees to 1230 degrees C as evident from the consistent gloss values of glazes (92-95 GU) and matching thermal expansion values.

Author
A T Achuthan & K N Maiti
Origin
Naroda Centre, Ahmedabad
Journal Title
Trans Indian Ceramic Soc 66 2 Apr-June 2007
Sector
Enamels
Class
E 158

Request article (free for British Glass members)

Examination Of Industrial Practice Of Ceramic Glaze Making With Emphasis On Particle Size Distribution
Trans Indian Ceramic Soc 66 2 Apr-June 2007
E 158
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 18 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.