The Evolution Of Gases In Bubbles In Molten Glass

The determination of the origin of a bubble from its gaseous content is complicated by the interaction between the bubble and the melt. In order to study this interaction a molten soda-lime-silica glass has been bubbled with air, nitrogen, oxygen, carbon dioxide, argon and sulfur dioxide at 1470 deg C. The residual bubbles are characterized by a low pressure, heavy sulfur/sulfate deposits and very similar compositions (N2 and CO2). In particular, bubbling with oxygen produces bubbles with constant PN2 and PCO2 indicating that an equilibirum is reached.

Author
M Chopinet Et Al
Origin
Saint Gobain Recherche, France
Journal Title
Xvii Int Cong Glass Beijing, October 1995 252-257
Sector
General
Class
G 1789

Request article (free for British Glass members)

The Evolution Of Gases In Bubbles In Molten Glass
Xvii Int Cong Glass Beijing, October 1995 252-257
G 1789
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 10 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.