Evidence Of Secondary-Phase Seperation In An Alkali Borosilicate Glass

This communication presents evidence that secondary phase seperation occurs as a result of the heat treatment step.

Author
J A Ruller, E J Friebele
Origin
Naval Research Laboratory, Usa
Journal Title
J Am Ceram Soc 1992 75 4 1026-27