Evaporation From Lead Silicate Melts In Dry And Wet Carbon Dioxide Atmosphere

Vaporisation from silicate melts containing PbO was studied by determining the total weight loss following heat treatment of samples of binary glass PbO-Si02, ternary glass K20-Pb0-Si02 and a multi-component commercial crystal glass. The effects of temperature, time and partial pressure of water vapour in flowing atmosphere of carbon dioxide on the vaporisation losses were established. It was found that the vaporisation from all three types of glass melts was decisively affected by temperature.

Author
J Matousek & T Janu
Origin
Inst Chemical Technol, Czech Republic
Journal Title
Glass Technology 43C 2002 63-66
Sector
Special Glass
Class
S 2553

Request article (free for British Glass members)

Evaporation From Lead Silicate Melts In Dry And Wet Carbon Dioxide Atmosphere
Glass Technology 43C 2002 63-66
S 2553
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.