Evaluation Of Some Factors In The Forming Of Glass Products

The changes in physico-chemical properties and characteristics of the glasses when different types of forming are used are discussed in relation to forming under both isothermal and non-isothermal conditions.

Author
Yu A Guloyan
Origin
Unknown
Journal Title
Glass And Ceramics 1989 46 5-6 240-244