Evaluation Of Phosphorous Concentration And Its Effect On Iscous Flow And Reflow In Phosphosilicate Glass.

Describes the use of x-ray fluorescence. By comparison with other available methods, we shall demonstrate that this direct measurement technique is accurate, simple, fast, reproducible, and nondestructive. With the use of this technique, flow and reflow profiles of phosphosilicate glass will be illustrates at different phosphorous concentrations and representative thermal cycles.

Author
R.A. Levy Et Al.
Origin
Unknown
Journal Title
J. Electrochem. Soc., 1985, 132 (6) 1472-9
Sector
Primary Papers
Class
PP 568

Request article (free for British Glass members)

Evaluation Of Phosphorous Concentration And Its Effect On Iscous Flow And Reflow In Phosphosilicate Glass.
J. Electrochem. Soc., 1985, 132 (6) 1472-9
PP 568
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.