Evaluation Of Mechanical Stability Of A Commercial Sn88 Silicon Nitride At Intermediate Temperatures

Dynamic fatigue and stress rupture tests in four-point bending were conducted on a commercially available SN88 silicon nitride ceramic at temperatures in the range 700-1000 deg C in air. The objective of the study was to elucidate the failure of SN88 silicon nitride ceramic nozzles arising from a critical crack initiated at the intermediate temperature airfoil region during an engine field test. Results of dynamic fatigue tests indicated that SN88 silicon nitride tested at a stressing rate of 30 MPa/s exhibited little change in characteristic strength at the various test temperatures.

Author
H Lin Et Al
Origin
Oak Ridge Nat Labs, Usa
Journal Title
Jacs 86 7 2003 1176-1181
Sector
Glass Ceramics
Class
GC 530

Request article (free for British Glass members)

Evaluation Of Mechanical Stability Of A Commercial Sn88 Silicon Nitride At Intermediate Temperatures
Jacs 86 7 2003 1176-1181
GC 530
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
12 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.