Evaluation Of The Influence Of Water In Glass On The Forming Behaviour Of Container Glass With The Help Of A Mathematical Model

The container forming process is simulated with a mathematical model. To highlight the relative influence of glass colour, OH level and bottle thickness, a container with a given shape is prodcued with eight combinations of green and white glass, high and low OH content, thin and thick wall starting from equal initial conditions. The influence of the variables considered ranged in the sequence: colour> thickness> OH content. The infleunce of OH level on timing and temperature profiles was appreciable for a water content differnece of 300ppm. The differences can be expected to be neglibible for daily oscillations of the order of 25ppm.

Author
R Dall'Igna & F Geotti-Bianchini
Origin
Stazione Sperimental, Italy
Journal Title
Int Glass Journal No 102 1999 57-62
Sector
Container glass
Class
C 1506

Request article (free for British Glass members)

Evaluation Of The Influence Of Water In Glass On The Forming Behaviour Of Container Glass With The Help Of A Mathematical Model
Int Glass Journal No 102 1999 57-62
C 1506
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 12 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.