Evaluation Of Crack Growth In Glass By Using Stress-Wave Fractography

Subcritical crack growth in glass shows three characteristic regions, depending on crack velocity. Among three regions, in region III, where water does not affect crack-growth behaviour, the slope of the crack-growth curve can be correlated with the intrinsic nature of glass fracture. In this study, to measure the crack velocity in region III, a periodic stress wave was applied to produce fracture-surface markings in the double-cleavage-drilled compression specimen. The crack-growth data obtained were compared with results obtained via direct observation of the crack front. As a result, this method, by using stress-wave fractography, was found to be effective to obtain the crack-growth curve in region III.

Author
S Yoshida Et Al
Origin
University Of Shiga, Japan
Journal Title
J Am Ceram Soc 82 6 1999 1621-1623
Sector
Special Glass
Class
S 1667

Request article (free for British Glass members)

Evaluation Of Crack Growth In Glass By Using Stress-Wave Fractography
J Am Ceram Soc 82 6 1999 1621-1623
S 1667
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.